tag:blogger.com,1999:blog-2131958746786008795.post5035207002169666291..comments2024-01-24T11:52:22.915-05:00Comments on playing with bits: Faster PCB Etching with Ferric ChlorideBradhttp://www.blogger.com/profile/13205011980298945921noreply@blogger.comBlogger5125tag:blogger.com,1999:blog-2131958746786008795.post-77848287683057302062013-01-04T22:03:42.326-05:002013-01-04T22:03:42.326-05:00I don't get it. What does the vortexer do? D...I don't get it. What does the vortexer do? Does it just make the glass dish vibrate? Or does it tilt it up and down from side to side, or what? I've been looking to do something like this myself.<br /><br />Thanks,<br />MikeAnonymoushttps://www.blogger.com/profile/08925851672644559702noreply@blogger.comtag:blogger.com,1999:blog-2131958746786008795.post-78290676542315946542012-10-21T02:09:31.689-04:002012-10-21T02:09:31.689-04:00This is really a great and useful piece of info. I...This is really a great and useful piece of info. I am glad to visit your blog. Please keep us up to date like this. Thank you for sharing.<br /><a href="http://www.rushpcb.com/PCB/flexcircuit.aspx" rel="nofollow">Flexible PCB</a><br />Anonymousnoreply@blogger.comtag:blogger.com,1999:blog-2131958746786008795.post-47409834116953329002012-01-06T23:32:20.762-05:002012-01-06T23:32:20.762-05:00Are you diluting with 2 parts water? I noticed so...Are you diluting with 2 parts water? I noticed some sites that said that this would cut down etching time by quite a bit.<br /><br />JimAnonymoushttps://www.blogger.com/profile/12744938692849246661noreply@blogger.comtag:blogger.com,1999:blog-2131958746786008795.post-50028219065218965592011-09-06T07:40:05.642-04:002011-09-06T07:40:05.642-04:00Google contact etching.Google contact etching.Perrowhttps://www.blogger.com/profile/09224950097186931426noreply@blogger.comtag:blogger.com,1999:blog-2131958746786008795.post-23496789425887584452011-03-31T23:12:08.411-04:002011-03-31T23:12:08.411-04:00Nice! I've recently taking to heating my FeCl...Nice! I've recently taking to heating my FeCl container in a water bath inside my reflow skillet at about 120-160°F. Last board I did etched in about 20 minutes. Now the challenge is getting them out fast enough so they don't over-etch. :) I wonder how hard it would be to make an agitator DIY-like?Mike Shimniokhttps://www.blogger.com/profile/17602015624941667574noreply@blogger.com